Description

Chemical Composition (%)

C Mn P S Si Cr Ni N
≤0.15 5.5-7.5 ≤0.060 ≤0.030 ≤1.00 16.0-18.0 3.5-5.5 ≤0.25

Mechanical Properties (Annealed)

Tensile Strength Yield Strength Elongation Hardness
≥515 MPa ≥275 MPa ≥40% ≤217 HB

Physical Properties

Density Melting Point Thermal Expansion Thermal Conductivity Elastic Modulus
7.93 g/cm³ 1400-1450°C 16.0 μm/m·°C 16.2 W/m·°C 195 GPa

201 Stainless Steel Pipe

Specifications & Applications: Cost-effective Cr-Ni-Mn austenitic stainless steel pipe; Mn replaces Ni to lower cost while offering good strength and formability for tubular applications. Applications: Ornamental tubing, structural piping, light-duty fluid lines, furniture, handrails

Chemical Composition (%)

C Mn P S Si Cr Ni N
≤0.15 5.5-7.5 ≤0.060 ≤0.030 ≤1.00 16.0-18.0 3.5-5.5 ≤0.25

Mechanical Properties (Annealed)

Tensile Strength Yield Strength Elongation Hardness
≥515 MPa ≥275 MPa ≥40% ≤217 HB

Physical Properties

Density Melting Point Thermal Expansion Thermal Conductivity Elastic Modulus
7.93 g/cm³ 1400-1450°C 16.0 μm/m·°C 16.2 W/m·°C 195 GPa