Chemical Composition (wt %, max unless range given)
C Mn P S Si Cr Ni N
<=0.15 <=2.00 <=0.045 <=0.030 <=1.00 17.0-19.0 8.0-10.0 <=0.10
Mechanical Properties (annealed tube)
Tensile Strength Yield Strength Elongation Reduction of Area Hardness
>=515 MPa >=205 MPa >=40 % >=50 % <=217 HB
Physical Properties (typical)
Density Melting Point Thermal Expansion Thermal Conductivity Modulus of Elasticity
8.03 g/cm3 1399-1421 °C 17.3 μm/m·°C 16.2 W/m·°C 193 GPa

302 Stainless Steel Coil

General-purpose Cr-Ni austenitic stainless steel coil; balanced overall performance; excellent corrosion resistance and deep-drawability for kitchen and architectural panels.

Chemical Composition (wt %, max unless range given)
C Mn P S Si Cr Ni N
<=0.15 <=2.00 <=0.045 <=0.030 <=1.00 17.0-19.0 8.0-10.0 <=0.10
Mechanical Properties (annealed tube)
Tensile Strength Yield Strength Elongation Reduction of Area Hardness
>=515 MPa >=205 MPa >=40 % >=50 % <=217 HB
Physical Properties (typical)
Density Melting Point Thermal Expansion Thermal Conductivity Modulus of Elasticity
8.03 g/cm3 1399-1421 °C 17.3 μm/m·°C 16.2 W/m·°C 193 GPa