Description

Chemical Composition (wt %, max unless range given)
C Mn P S Si Cr
<=0.15 <=1.00 <=0.040 <=0.030 <=1.00 11.5-13.5
Mechanical Properties (annealed tube)
Tensile Strength Yield Strength Elongation Hardness
>=485 MPa >=275 MPa >=20 % <=200 HB
Physical Properties (typical)
Density Melting Point Thermal Expansion Thermal Conductivity Modulus of Elasticity
7.70 g/cm3 1480-1530 °C 11.0 μm/m·°C 25.0 W/m·°C 200 GPa

410 Stainless Steel Coil

Basic martensitic stainless steel coil; chromium content 11.5-13.5%; can obtain high strength and hardness through heat treatment; good wear resistance for cutter shims and blade stock.

Chemical Composition (wt %, max unless range given)
C Mn P S Si Cr
<=0.15 <=1.00 <=0.040 <=0.030 <=1.00 11.5-13.5
Mechanical Properties (annealed tube)
Tensile Strength Yield Strength Elongation Hardness
>=485 MPa >=275 MPa >=20 % <=200 HB
Physical Properties (typical)
Density Melting Point Thermal Expansion Thermal Conductivity Modulus of Elasticity
7.70 g/cm3 1480-1530 °C 11.0 μm/m·°C 25.0 W/m·°C 200 GPa