Description

Chemical Composition (wt %, max unless range given)
C Mn P S Si Cr
<=0.15 <=1.25 <=0.060 >=0.15 <=1.00 12.0-14.0
Mechanical Properties (annealed tube)
Tensile Strength Yield Strength Elongation Hardness
>=485 MPa >=275 MPa >=20 % <=200 HB
Physical Properties (typical)
Density Melting Point Thermal Expansion Thermal Conductivity Modulus of Elasticity
7.70 g/cm3 1480-1530 °C 11.0 μm/m·°C 25.0 W/m·°C 200 GPa

416 Stainless Steel Plate

Free-machining martensitic stainless steel plate; added phosphorus and sulfur elements; excellent machinability for intricate machined parts but relatively lower corrosion resistance.

Chemical Composition (wt %, max unless range given)
C Mn P S Si Cr
<=0.15 <=1.25 <=0.060 >=0.15 <=1.00 12.0-14.0
Mechanical Properties (annealed tube)
Tensile Strength Yield Strength Elongation Hardness
>=485 MPa >=275 MPa >=20 % <=200 HB
Physical Properties (typical)
Density Melting Point Thermal Expansion Thermal Conductivity Modulus of Elasticity
7.70 g/cm3 1480-1530 °C 11.0 μm/m·°C 25.0 W/m·°C 200 GPa