Description

Chemical Composition (wt %, max unless range given)
Ni Cr Mo Nb Fe C Mn Si Al Ti
Balance 20.0-23.0 8.0-10.0 3.15-4.15 <=5.0 <=0.10 <=0.5 <=0.5 <=0.4 <=0.4
Mechanical Properties (annealed tube)
Tensile Strength Yield Strength Elongation Hardness
>=830 MPa >=415 MPa >=30 % <=220 HB
Physical Properties (typical)
Density Melting Point Thermal Expansion Thermal Conductivity Modulus of Elasticity
8.44 g/cm3 1290-1350 °C 12.8 μm/m·°C 9.8 W/m·°C 208 GPa

Inconel 625 Nickel‑Base High‑Temperature Alloy Plate

Nickel-chromium-molybdenum-niobium solid-solution strengthened superalloy plate; solid-solution strengthening from molybdenum and niobium provides excellent tensile strength and creep resistance; outstanding salt spray corrosion resistance for submarine hull sections.

Chemical Composition (wt %, max unless range given)
Ni Cr Mo Nb Fe C Mn Si Al Ti
Balance 20.0-23.0 8.0-10.0 3.15-4.15 <=5.0 <=0.10 <=0.5 <=0.5 <=0.4 <=0.4
Mechanical Properties (annealed tube)
Tensile Strength Yield Strength Elongation Hardness
>=830 MPa >=415 MPa >=30 % <=220 HB
Physical Properties (typical)
Density Melting Point Thermal Expansion Thermal Conductivity Modulus of Elasticity
8.44 g/cm3 1290-1350 °C 12.8 μm/m·°C 9.8 W/m·°C 208 GPa