Description

Chemical Composition (wt %, max unless range given)
C Mn P S Si Cr Ni Mo N
<=0.08 7.5-9.0 <=0.045 <=0.030 <=0.75 17.5-22.0 5.0-7.0 2.00-3.00 0.25-0.50
Mechanical Properties (annealed tube)
Tensile Strength Yield Strength Elongation Hardness
>=620 MPa >=310 MPa >=40 % <=217 HB
Physical Properties (typical)
Density Melting Point Thermal Expansion Thermal Conductivity Modulus of Elasticity
7.93 g/cm3 1398-1446 °C 16.8 μm/m·°C 15.8 W/m·°C 195 GPa

XM-17 Stainless Steel Bar

High-strength nitrogen-alloyed austenitic stainless steel bar; combination of high manganese, nitrogen, and molybdenum provides excellent strength and corrosion resistance for drill collars and sub-sea connectors.

Chemical Composition (wt %, max unless range given)
C Mn P S Si Cr Ni Mo N
<=0.08 7.5-9.0 <=0.045 <=0.030 <=0.75 17.5-22.0 5.0-7.0 2.00-3.00 0.25-0.50
Mechanical Properties (annealed tube)
Tensile Strength Yield Strength Elongation Hardness
>=620 MPa >=310 MPa >=40 % <=217 HB
Physical Properties (typical)
Density Melting Point Thermal Expansion Thermal Conductivity Modulus of Elasticity
7.93 g/cm3 1398-1446 °C 16.8 μm/m·°C 15.8 W/m·°C 195 GPa